The effect of reactor temperature and hydrogen flow rate on carbon nanofibers (CNFs) characterizations and their adsorption capacity
Helical and straight CNFs are prepared using Floating Catalyst- Chemical Vapor Deposition (FC-CVD) from decomposition of ethanol as carbon source, hydrogen as carrier gas and argon as purge gas. The effect of reactor temperature (700 - 950°C) and hydrogen flow rate (100 - 350 mL/min) on BET surface...