Modification of oil palm mesocarp fiber characteristics using superheated steam treatment
In this study, oil palm mesocarp fiber (OPMF) was treated with superheated steam (SHS) in order to modify its characteristics for biocomposite applications. Treatment was conducted at temperatures 190–230 °C for 1, 2 and 3 h. SHS-treated OPMF was evaluated for its chemical composition, thermal stabi...