Synthesis and characterization of CdSe nanoparticles via thermal treatment technique

The synthesis of CdSe nanoparticles was undertaken via the thermal treatment method at varying calcination temperatures from 450 to 700 °C in alternate oxygen and nitrogen environment. Selenium powder was dissolved in ethylenediamine at 200 °C for 2 h before mixing with the metal precursor, cadmium...